Type 410 Stainless
(UNS S41000)
Single Figures are Maximums
0.15 C, 1.00 Mn, 0.040 P, 0.030 S, 1.00 Si, 11.50/13.00 Cr, Bal. Fe
Hardenable martensitic stainless alloy used for highly stressed parts needing good corrosion resistance and strength. Can be heat-treated to obtain high-strength properties with good ductility.
Register/log in to our Tech Center for detailed technical alloy datasheets on more than 200 Carpenter specialty metals. The database is searchable and free.