(UNS S30200)
Single Figures are Maximums
0.15 C, 2.00 Mn, 0.045 P, 0.03 S, 1.00
Si, 17.00/19.00 Cr, 8.00/10.00 Ni, Bal. Fe
Austenitic, nonmagnetic, extremely tough and ductile, this is
one of the most widely used of the chrome-nickel stainless and heat-resisting
steels. Nonhardenable by heat treating.
 |
Use our
Technical Information database to get comprehensive
technical data on hundreds of Carpenter alloys. The database is
searchable and it's free. |
| Copyright 1997-2008 CRS Holdings Inc. All
rights reserved. |
|