Single Figures are Maximums
0.2 C, 2.0 Mn, 0.5 Si, 0.015 S, 63.0/70.0 Ni, 2.50 Fe, Bal. Cu
A nickel-copper solid solution alloy which has been used up to 800°F (427°C)
in a variety of applications, including chemical processing and marine applications.
Alloy can be strengthened by cold working.
 |