| Carpenter Low Expansion "45" Alloy |
Nominal Analysis
0.05 C, 0.4 Mn, 0.25 Si, 45.00 Ni, Bal. Fe
This alloy has a relatively constant rate of thermal expansion to
about 800°F (538°C). It has been used in thermostats, and its
thermal expansion approximates that of some alumina ceramics.