(UNS N06625)
Single Figures are Maximums
0.10 C, 0.50 Mn, 0.50 Si, 0.015 P, 0.015 S, 20.0/23.0 Cr, 8.0/10.0 Mo, 5.00
Fe, 0.40 Ti, 1.00 Co, 3.15/4.15 Cb and Ta, 0.40 Al, Bal. Ni
Solid-solution-strengthened nickel-base alloy
that exhibits outstanding strength and toughness from cryogenic to 2000°F
(1093°C) temperature range. Has excellent fatigue strength and stress-corrosion
cracking resistance to chloride ions. Has been used for gas turbine engine components,
furnace hardware, chemical plant hardware, and sour brine applications.
 |