(UNS N19909)
Single Figures are Maximums Unless Otherwise Noted
0.06 C, 0.50 Mn, 0.40 nom. Si, 0.015 P, 0.015 S, 0.50 Cr, 38.00 nom. Ni, 14.00
nom. Co, 1.60 nom. Ti, 4.90 nom. Cb + Ta, 0.15 Al, 0.50 Cu, 0.012 B, Bal. Fe
A high-strength, precipitation-hardenable superalloy which exhibits
a low and relatively constant coefficient of thermal expansion over a broad
temperature range, high hot hardness and good thermal fatigue resistance. Offers
significant improvement over Pyromet alloys CTX-1 and CTX-3 due to its excellent
combination of tensile properties and stress rupture strength to 1200°F (649°C)
in the recrystallized condition combined with the use of common age hardening
treatments. This alloy requires a protective coating if exposed to atmospheric
conditions above 1000°F (538°C).
 |
Use our
Technical Information database to get comprehensive
technical data on hundreds of Carpenter alloys. The database is
searchable and it's free. |